Beschreibung
Merkmale:
It is austenitic stainless steel filler metal for welding of 18%Cr-12%Ni-2%Mo types. The molybdenum increased pitting corrosion resistance. The low carbon content improved intergranular corrosion.
Anwendungen:
Typical applications include welding of 18%Cr-12%Ni-2%Mo stainless steel in chemical, oil and gas refineries.
Hinweise zur Verwendung:
- Use Spray Transfer or Short Circuit Transfer mode.
- 98%Argon – 2%O₂ shielding gas is recommended.
Einstufung:
AWS A5.9 ER316L
JIS Z3321 Y316L
Typische chemische Zusammensetzung des Schweißguts (wt%)
| C | Cr | Ni | Mo | Si | Mn |
| 0.023 | 19.60 | 13.1 | 2.30 | 0.5 | 1.45 |
Typische mechanische Eigenschaften des Schweißguts
| TS N/mm2 | EL % |
| 580 | 40 |
Sizes and Gewicht pro Packung.
| Durchmesser (mm) | 0.8 | 0.9 | 1.0 | 1.2 |
| Gewicht pro Packung (kg) | 12.5 | 12.5 | 12.5 | 12.5 |