Deskripsi
Karakteristik:
Provides a fully austenitic weld metal and is therefore somewhat more sensitive to hot cracking than 316 grades. Welding should be performed with low heat input, interpass temperature and dilution with parent metal.
Aplikasi:
It is suitable for joining and surfacing of matching / similar heat resistant steels / cast steel grades, ferritic chromium steels, 14 %-Mn steels.
Catatan tentang Penggunaan:
1. Use 100% CO₂ shielding gas.
2. Use DC(+) polarity.
3. Trailer Shield is required to ensure the weld pool completely shield until solidi ication is complete and no porosity problem.
4. To get enough penetration in the down hand welding position recommend maintaining a higher welding speed.
Klasifikasi:
AWS A5.22 E310LT1-1
Welding Position:

Komposisi kimiawi khas logam las (wt%)
| C | Mn | Si | P | S | Cr | Ni | Mo |
| 0.054 | 2.15 | 0.71 | 0.015 | 0.006 | 25.9 | 21-18 | 0.46 |
Sifat mekanis khas dari logam las
| TS N/mm² | EL % |
| 570 | 36 |
Ukuran dan rentang arus yang disarankan (DC+)
| Diameter (mm) | 1.2 | |||
| Posisi Pengelasan | F, HF | H | V-UP | OH |
| Tegangan (Volt) | 24-33 | 25-29 | 24-28 | 25-29 |
| Arus (Amp) | 130-220 | 140-180 | 130-160 | 150-180 |
| Menonjol (mm) | 15-20 | 15-20 | 15-20 | 15-20 |
| Laju aliran (l/menit) | 20-25 | 20-25 | 20-25 | 20-25 |
| Berat per gulungan (kg) | 12.5 | |||