Stainless Steel Electrodes LKE-NiCrMo-10

Beschreibung

Merkmale:

Good corrosion-resistance against acetic acid and its anhydride, hot contaminated sulphuric and phosphoric acids and other contaminated oxidizing mineral acids. Intermetallic precipitation is widely prevented.

Anwendungen:

For joining materials of the same and similar nature, e.g. material-no. 2.4602 (NiCr21Mo14W / UNS N06022) and special stainless steels. Furthermore it can be used for dissimilar joints of these alloys with low-alloyed materials and cladding

Hinweise zur Verwendung:

1.Dry the electrode at 350-400°C for 60 minutes before use.
2. halten Sie den Lichtbogen so kurz wie möglich.
3.Crater should be ground smooth or crater treatment.

Einstufung:

AWS A5.11 ENiCrMo-10

Position beim Schweißen:

Typische chemische Zusammensetzung des Schweißguts (wt%)

C Mn Si Cr Mo Ni S W Fe
0.018 0.28 0.19 22.47 14.00 54.26 0.002 3.21 5.14

Typische mechanische Eigenschaften des Schweißguts

TS N/mm² EL % IV -30°C J
770 40 70

Größen und empfohlener Strombereich (AC oder DC+)

Durchmesser (mm) 2.6 3.2 4.0 4.8
Länge (mm) 300 350 350 350
Ampere F 90-120 120-160 160-220 230-300
V&OH 70-110 80-120 110-150 230-300
Gewicht pro Packung (kg) 5 5 5 5
Gewicht pro Karton (kg) 20 20 20 20