Description
Caractéristiques :
Good corrosion-resistance against acetic acid and its anhydride, hot contaminated sulphuric and phosphoric acids and other contaminated oxidizing mineral acids. Intermetallic precipitation is widely prevented.
Applications :
For joining materials of the same and similar nature, e.g. material-no. 2.4602 (NiCr21Mo14W / UNS N06022) and special stainless steels. Furthermore it can be used for dissimilar joints of these alloys with low-alloyed materials and cladding
Notes sur l'utilisation :
1.Dry the electrode at 350-400°C for 60 minutes before use.
2.Keep the arc as short as possible.
3.Crater should be ground smooth or crater treatment.
Classification :
AWS A5.11 ENiCrMo-10
Position de soudage :

Composition chimique typique du métal soudé (wt%)
| C | Mn | Si | Cr | Mo | Ni | S | W | Fe |
| 0.018 | 0.28 | 0.19 | 22.47 | 14.00 | 54.26 | 0.002 | 3.21 | 5.14 |
Propriétés mécaniques typiques du métal soudé
| TS N/mm² | EL % | IV -30°C J |
| 770 | 40 | 70 |
Dimensions et plage de courant recommandée (AC ou DC+)
| Diamètre (mm) | 2.6 | 3.2 | 4.0 | 4.8 | |
| Longueur (mm) | 300 | 350 | 350 | 350 | |
| Ampères | F | 90-120 | 120-160 | 160-220 | 230-300 |
| V&OH | 70-110 | 80-120 | 110-150 | 230-300 | |
| Poids par paquet (kg) | 5 | 5 | 5 | 5 | |
| Poids par carton (kg) | 20 | 20 | 20 | 20 | |