Deskripsi
Karakteristik:
Good corrosion-resistance against acetic acid and its anhydride, hot contaminated sulphuric and phosphoric acids and other contaminated oxidizing mineral acids. Intermetallic precipitation is widely prevented.
Aplikasi:
For joining materials of the same and similar nature, e.g. material-no. 2.4602 (NiCr21Mo14W / UNS N06022) and special stainless steels. Furthermore it can be used for dissimilar joints of these alloys with low-alloyed materials and cladding
Catatan tentang Penggunaan:
1.Dry the electrode at 350-400°C for 60 minutes before use.
2. Jaga agar busur sependek mungkin.
3.Crater should be ground smooth or crater treatment.
Klasifikasi:
AWS A5.11 ENiCrMo-10
Posisi pengelasan:

Komposisi kimiawi khas logam las (wt%)
| C | Mn | Si | Cr | Mo | Ni | S | W | Fe |
| 0.018 | 0.28 | 0.19 | 22.47 | 14.00 | 54.26 | 0.002 | 3.21 | 5.14 |
Sifat mekanis khas dari logam las
| TS N/mm² | EL % | IV -30°C J |
| 770 | 40 | 70 |
Ukuran dan kisaran arus yang disarankan (AC atau DC+)
| Diameter (mm) | 2.6 | 3.2 | 4.0 | 4.8 | |
| Panjang (mm) | 300 | 350 | 350 | 350 | |
| Amps | F | 90-120 | 120-160 | 160-220 | 230-300 |
| V & OH | 70-110 | 80-120 | 110-150 | 230-300 | |
| Berat per kemasan (kg) | 5 | 5 | 5 | 5 | |
| Berat per karton (kg) | 20 | 20 | 20 | 20 | |